Beginners Guide to TikTok for Search - Rachel Pearson - We are Tilt __ Bright...
Nanoindentation Of Pharmaceutical Crystals
1. A systematic method to study slip planes in molecular crystals by nanoindentation Yuanyuan Jing1, Yan Zhang2, John Blendell1, Marisol Koslowski3* and M. Teresa. Carvajal2,4* 1.School of Materials Engineering, 2.Industrial and Physical Pharmacy, 3.Mechanical Engineering, 4. Agricultural and Biological Engineering, Purdue University, West Lafayette, IN 47906-2093
2. b̅ c̅ Slip trace ӨTrace Reference direction 115.9o a̅